Using state-of-the-art lamination technology, MicroGuard MP® Microporous Shoe Covers combine a soft, non-woven fabric with a microporous film. A tear-resistant liquid and particulate barrier helps safeguard from blood penetration, various industrial chemicals, along with dust, dirt, and grime. This breathable fabric allows moisture to escape, so your feet are more cool and comfortable even as you sweat. These shoe covers come with a strong elastic closure at the top to keep them in place and they are also environmentally friendly.
- Feature 1Elastic top for snug, secure fit.
- Feature 2Environmentally friendly—can be recycled after use
Details
Protection agent | Dry particulates, Over-spray |
---|---|
Size | L |
Pack Type | Bulk |
Sterile | No |
Color | White |
Material | Microporous Fabric |
Seam Style | Serged Seams |
Closure Type | Latex Free Elastic |
Country of Origin | China |
UPC | 813383011026 |
Physical Properties
Test | Method | Result |
---|---|---|
Fabric Weight (oz/y²) | ASTM D3776 | 1.6 |
Water Vapor Trasmission (g/m2/24h) | GB/T 12074-1991 | 3200 |
Water Resistance (Kpa) | FZ/T 01004-1991 | 18.8 |
Flat Abrasion | FZ/T 01001-1991 | 198 |
Breaking Strength (N/5cm) | GB/T 3923.1-1997 | Radial: 70 / Woof: 50 |
Elongation at Break (%) | GB/T 3923.1-1997 | Radial: 60 / Woof: 50 |
Tear Strength (N/5cm) | ASTM D2261-1996 | Sample cut horizontally, normal testing cannot be done. Woof: 8.6 |
Electric Charge Density (uC/m2) | GB/T 5455-1997 | 6.5 |
Flammability | GB/T 4744-1997 | Melt-down |
Dry particle Filtration Efficiency | ASTM F 2299 | No Particle Penetration |
Wet Particle Filtration Efficiency | ASTM F 2299 | No Particle Penetration |
Air Permeability (cfm) | ASTM D737 | <0.55 |
Burst Strength (lbs) | ASTM D3787 | 20 |
Tensile Strength (lbs) Machine Direction | ASTM D5034 | 23.2 |
Tensile Strength (lbs) Cross Direction | ASTM D5034 | 18.1 |
Tensile Strength (lbs) Trapezoidal - Machine Direction | ASTM D1117 | 9.76 |
Tensile Strength (lbs) Trapezoidal - Cross Direction | ASTM D1117 | 4.97 |
BS EN 1149-1:2006 Surface Resistivity
BS EN 1149-1:2006 Protective clothing. Electrostatic properties- Test method for measurement of surface resistivity. Surface resistance= 1.2 x 109 Ω
Liquid and Chemical Resistance
Test | Method | Result |
---|---|---|
Bleach 5% | ASTM F903 | Pass |
Hydraulic Jack Oil | ASTM F903 | Pass |
Isocyanate Based Paint Hardener | ASTM F903 | Pass |
Motor Oil | ASTM F903 | Pass |
Sodium hydroxide | ASTM F903 | Pass |
Mineral Oil | ASTM F903 | Pass |
Blood | ASTM 1670-07 | Pass |